Particle atomic layer deposition of alumina for sintering yttria-stabilized cubic zirconia
Rebecca J. O'Toole, Christopher J. Bartel, Maila U. Kodas, Alexa J. Horrell, Sandrine Ricote, Neal P. Sullivan, Christopher J. Gump, Charles B. Musgrave, Alan W. Weimer
Research output: Contribution to journal › Article › peer-review