On the discontinuous nature of stress-corrosion cracking in titanium alloys

Y. Katz, W. W. Gerberich

Research output: Contribution to journalArticlepeer-review

8 Scopus citations

Fingerprint

Dive into the research topics of 'On the discontinuous nature of stress-corrosion cracking in titanium alloys'. Together they form a unique fingerprint.