On the discontinuous nature of stress-corrosion cracking in titanium alloys

Y. Katz, W. W. Gerberich

Research output: Contribution to journalArticlepeer-review

8 Scopus citations
Original languageEnglish (US)
Pages (from-to)219-221
Number of pages3
JournalInternational Journal of Fracture Mechanics
Volume6
Issue number2
DOIs
StatePublished - Jun 1970
Externally publishedYes

Cite this