Nanoindentaion techniques for assessing mechanical reliability at the nanoscale

Alex A. Volinsky, William W Gerberich

Research output: Contribution to journalArticlepeer-review

72 Scopus citations

Fingerprint

Dive into the research topics of 'Nanoindentaion techniques for assessing mechanical reliability at the nanoscale'. Together they form a unique fingerprint.