MECHANICAL NATURE OF STRESS-CORROSION CRACKING IN Al-Zn-Mg ALLOYS - 1. EVALUATION OF THE DUCTILE RUPTURE CONTRIBUTION.

W. E. Wood, W. W. Gerberich

Research output: Contribution to journalArticlepeer-review

13 Scopus citations

Fingerprint Dive into the research topics of 'MECHANICAL NATURE OF STRESS-CORROSION CRACKING IN Al-Zn-Mg ALLOYS - 1. EVALUATION OF THE DUCTILE RUPTURE CONTRIBUTION.'. Together they form a unique fingerprint.