INHIBITIVE EFFECT OF OXYANIONS ON THE STRESS CORROSION CRACKING OF TYPE 304 STAINLESS STEEL IN BOILING 20N NaOH SOLUTION.

Y. S. Park, A. K. Agrawal, R. W. Staehle

Research output: Contribution to specialist publicationArticle