INHIBITIVE EFFECT OF OXYANIONS ON THE STRESS CORROSION CRACKING OF TYPE 304 STAINLESS STEEL IN BOILING 20N NaOH SOLUTION.

Y. S. Park, A. K. Agrawal, R. W. Staehle

Research output: Contribution to specialist publicationArticle

7 Scopus citations

Abstract

The effect of various oxyanions in inhibiting the stress corrosion cracking (SCC) of Type 304 stainless steel in boiling 20N NaOH was investigated. Times to failure of wire specimens were measured in the absence and in the presence of various oxyanions in the NaOH solution. Out of 16 oxyanions tested, CrO//4** equals was found to be the most effective in inhibiting the SCC of Type 304.