N2 - Solid contacts made of nonredox-active high-surface-area materials provide ion-selective electrodes comprising an ionophore-doped sensing membrane with a high capacitance. As emphasized in the literature, this minimizes changes in the measured potential that result from the minimal but unavoidable currents of real-life potentiometric measurements. However, as shown here for solid contacts made of single-walled carbon nanotubes (SWCNTs), solid contacts actively charged up over several minutes to voltages as small as ±100 mV do not hold this charge for longer than a few hours. Potential discharge occurs due to Faradaic processes and charge redistribution within the narrow confines of the SWCNT layer. The composition of the sensor membranes and atmospheric conditions have only a small impact on the kinetics of this spontaneous discharge, suggesting that redox reactions involving oxygen and the sensing membrane components do not play critical roles. Because both ion mobilities and the rate of redox reactions are expected to increase with temperature, the significant acceleration of discharge at higher temperature does not clarify whether charge redistribution or redox reactions dominate this discharge. However, contact angle measurements show that SWCNT-modified electrodes without an ion-selective membrane exhibit a substantial decrease in hydrophobicity after prolonged application of a bias potential as small as +100 mV, while application of a negative voltage had only a minor effect. This is consistent with very slow oxidation of the SWCNTs. These findings highlight the importance of optimizing the surface chemistry of high-surface-area solid contacts in view of high long-term stabilities. We propose quick charging of solid contacts to moderate potentials, followed by long-term potential monitoring under zero-current conditions, as a more thorough approach to characterize ISEs with high-surface-area solid contacts, offering insights not available with conventional chronopotentiometry measurements.
AB - Solid contacts made of nonredox-active high-surface-area materials provide ion-selective electrodes comprising an ionophore-doped sensing membrane with a high capacitance. As emphasized in the literature, this minimizes changes in the measured potential that result from the minimal but unavoidable currents of real-life potentiometric measurements. However, as shown here for solid contacts made of single-walled carbon nanotubes (SWCNTs), solid contacts actively charged up over several minutes to voltages as small as ±100 mV do not hold this charge for longer than a few hours. Potential discharge occurs due to Faradaic processes and charge redistribution within the narrow confines of the SWCNT layer. The composition of the sensor membranes and atmospheric conditions have only a small impact on the kinetics of this spontaneous discharge, suggesting that redox reactions involving oxygen and the sensing membrane components do not play critical roles. Because both ion mobilities and the rate of redox reactions are expected to increase with temperature, the significant acceleration of discharge at higher temperature does not clarify whether charge redistribution or redox reactions dominate this discharge. However, contact angle measurements show that SWCNT-modified electrodes without an ion-selective membrane exhibit a substantial decrease in hydrophobicity after prolonged application of a bias potential as small as +100 mV, while application of a negative voltage had only a minor effect. This is consistent with very slow oxidation of the SWCNTs. These findings highlight the importance of optimizing the surface chemistry of high-surface-area solid contacts in view of high long-term stabilities. We propose quick charging of solid contacts to moderate potentials, followed by long-term potential monitoring under zero-current conditions, as a more thorough approach to characterize ISEs with high-surface-area solid contacts, offering insights not available with conventional chronopotentiometry measurements.
KW - Charge Redistribution Mechanism
KW - Faradaic Processes
KW - Ion-Selective Electrodes
KW - Self-Discharge Dynamics
KW - Single-Walled Carbon Nanotubes
KW - Solid-Contact Interfaces
UR - http://www.scopus.com/inward/record.url?scp=105001230061&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=105001230061&partnerID=8YFLogxK
U2 - 10.1021/acssensors.4c03702
DO - 10.1021/acssensors.4c03702
M3 - Article
C2 - 40152660
AN - SCOPUS:105001230061
SN - 2379-3694
JO - ACS Sensors
JF - ACS Sensors
ER -