Analysis of stress corrosion crack-tip surface chemistries in 7075 type aluminum alloys

E. C. Pow, W. W. Gerberich, L. E. Toth

Research output: Contribution to journalArticle

7 Scopus citations
Original languageEnglish (US)
Pages (from-to)55-60
Number of pages6
JournalScripta Metallurgica
Volume15
Issue number1
DOIs
StatePublished - Jan 1981

Cite this